Project Description
DuraDestruct RFID Tags – Plastic
T his patent-pending RFID security tag product combines the durability of our standard RFID tag with destructible features that render the label useless if it is removed or tampered with. Its specialized construction eliminates the transferability of the RFID tag and incorporates two levels of destructibility. If someone attempts to remove the tag the RFID antenna construction breaks into separate pieces making the read range of the tag mere inches. If a person tries to reassemble the tag to make it functional, the portion that is still adhered to will literally disintegrate if an attempt is made to remove it from the object.
The plastic surface mount DuraDestruct UHF RFID tags are part of the DuraDestruct line of tamper/security tags that also includes glass surface mount RFID tags.
| Standard Size | Type |
|---|---|
| 101 × 25 × 0.44 mm | UHF |
Ideal for security and tamper proof RFID applications
Deters transferability as tag is rendered useless upon removal
Provides additional levels of security for RFID anti-theft and RFID protection systems
Perfect for plastic bins, totes, tubs and crates
Read range up to 12 metres on plastic
Custom printing available
Patent pending product
| Material | Polyester |
| Serialization | Bar code and human-readable equivalent are produced using the latest high-resolution digital technology available, which provides excellent clarity and easy scanning. Code 39 is the standard symbology with a range of 2.7 to 5.4 CPI (characters per inch). Optional symbology is Code 128. |
| Label Copy | The label copy may include block type, stylized type, logos or other designs |
| Colors | Standard colors include black, red, yellow, green, dark blue, orange, purple or blue. Custom spot colors are also available at no additional charge. Due to contrast needed for the bar code scanner, all bar codes are black. |
| Standard Adhesive | Pressure-sensitive acrylic adhesive |
| Frequency Range | Worldwide UHF RFID Operation (840 – 960 MHz) |
| Sizes | 101mm x 25mm |
| Packaging | Produced and shipped in roll form |
| Shipment | 14 business days |
Bins/Crates/Totes
Non-metal surfaces
Returnable Containers
Security applications
-
Chemical Testing
-
Temperature Testing
-
Read Range Testing
-
Abrasion Testing
Chemical Test Summary
Samples applied to glass panels, allowed to wet out for 72 hours, immersed in chemicals below at ambient room temperature conditions. Inlays in all samples still reading after 48 hours of exposure.
Key: NE = No effect; AO = adhesive ooze; PE = print erosion under laminate
Chemical Test Data
| Water | Salt Water 5% NaCI | Bathroom Cleaner | Glass Cleaner Windex Commercial Line | Isopropanol 99% | Brake Fluid DOT 3 | Acetone | Diesel Fuel | Nitric Acid pH 1.0 =/- 0.01 | Hydrochloric Acid pH 1.0 =/- 0.01 | Sodium Hydroxide pH 12.0 =/- 0.01 | |
| 2 hours | NE | NE | NE | NE | AO | AO | AO | AO | NE | NE | NE |
| 24 hours | NE | NE | NE | NE | AO | AO | AO | AO | NE | NE | NE |
| 48 hours | NE | NE | NE | PE | AO | AO | AO | AO | NE | NE | NE |
Temperature Test Data
| 93°C | 120°C | 150°C | 176°C | 204°C | 230°C | 260°C |
| NE | NE | NE | SS | TD, SS | TP, TD, SS | TM |
Read Range Test Data (metres)
DuraDestruct Voyanic Anechoic Chamber test results
| Substrate | ETSI | FCC |
|---|---|---|
| Windshield glass | 8.7 | 10.5 |
| Tempered glass | 8.2 | 9.2 |
| Polypropylene | 14.0 | 12.3 |
| HDPE | 11.5 | 15.4 |
| Wood | 9.3 | 9.0 |
| Corrugated Paper | 13.0 | 14.5 |
Abrasion Test Data
Tags survived 6,000 revolutions on Taber Abrader with CS-10 wheels, 1000g total load.